19-9 DL Stainless

UNS #K63198

19-9 DL stainless exhibits high strength and resistance to corrosion and oxidation at temperatures up to 1250°F (677°C). Like all austenitic alloys of this type, 19-9 DL cannot be strengthened by thermal treatment and is frequently used in the annealed condition. Higher properties can be achieved by hot-cold working. Specifications: AMS 5526 (Strip), AMS 5527 (Strip), AMS 5720 (Bars and Forgings), AMS 5721 (Bars and Forgings), AMS 5722 (Bars and Forgings)

Type Analysis

  • Carbon (Maximum) 0.28-0.35
  • Silicon (Maximum) 0.30-0.80
  • Nickel (Nominal) 9.00-11.00
  • Tungsten (Nominal) 1.00-1.75
  • Titanium (Nominal) 0.10-0.35
  • Manganese (Maximum) 0.75-1.50
  • Chromium (Nominal) 18.00-21.00
  • Molybdenum (Nominal) 1.00-1.75
  • Iron (Nominal) Balance
  • Columbium+Tantalum 0.25-0.60

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applications

Applicable Specifications

  • AMS 5526 (Strip)
  • AMS 5720 (Bars and Forgings)
  • AMS 5722 (Bars and Forgings)
  • AMS 5527 (Strip)
  • AMS 5721 (Bars and Forgings)

Bar

Rounds

Strip