Type Analysis

  • Carbon (Maximum) 0.03
  • Phosphorus (Maximum) 0.045
  • Silicon (Maximum) 1
  • Nickel (Nominal) 10.00-14.00
  • Manganese (Maximum) 2
  • Sulfur (Maximum) 0.03
  • Chromium (Nominal) 16.00-18.00
  • Molybdenum (Nominal) 2.00-3.00
  • Iron (Nominal) Balance
  • Nitrogen (Nominal) 0.10-0.16

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

  • ASTM A276
  • ASTM A182
  • ASTM A193
  • ASRM A194