600

UNS #N06600

600 is a nonmagnetic, nickel-base, high-temperature alloy possessing an excellent combination of high strength, hot and cold workability, and resistance to ordinary forms of corrosion. This alloy also displays good heat resistance and freedom from aging or stress corrosion throughout the annealed to heavily cold worked condition range.

Type Analysis

  • Carbon (Maximum) 0.1
  • Silicon (Maximum) 0.5
  • Nickel (Nominal) 72
  • Manganese (Maximum) 1
  • Sulfur (Maximum) 0.015
  • Chromium (Nominal) 14.00 - 17.00
  • Iron (Nominal) 6.00 - 10.00
  • Copper (Nominal) 0.5

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

  • AMS 5540
  • AMS 5665
  • AMS 5580
  • MIL-N-15721
  • MIL-N-22986
  • MIL-N-22987
  • MIL-N-23228
  • MIL-N-23229
  • MIL-N-6840
  • MIL-N-6710
  • QQ-W-390

Bar

Rounds

Billet

Strip

Wire

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.