9310

UNS #G93106

9310 VAC-ARC steel is a premium quality chromium-nickel-molybdenum carburizing steel produced by the vacuum consumable electrode process. It has high hardenability, high core hardness, and superior fatigue strength.

Type Analysis

  • Carbon (Nominal) 0.1
  • Phosphorus (Maximum) 0.025
  • Silicon (Nominal) 0.25
  • Nickel (Nominal) 3.25
  • Manganese (Nominal) 0.5
  • Sulfur (Maximum) 0.025
  • Chromium (Nominal) 1.2
  • Molybdenum (Nominal) 0.12
  • Iron (Nominal) Balance

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

  • AMS 6265
  • AMS 6267
  • MIL-S-7393
  • MIL-S-83030
  • BMS 7-249 (Boeing) (VIM-VAR)
  • HMS 6-1263 (Boeing-Mesa)
  • 299-947-032 (Bell) (VAR)
  • 299-947-302 (Bell) (VIM-VAR)
  • EMS 56279 (Honeywell)
  • EMS 56280 (Honeywell)
  • SS 9705 (Sikorsky) (VIM-VAR)

Bar

Rounds

Billet