PremoMet®

UNS #K63835

PremoMet® is a premium-melted, cobalt-free, high strength, high toughness quenched, and tempered alloy. It attains a typical 290 ksi (1999 MPa) UTS combined with a typical range of 60-65 ksi sqrt(in) (66-71 MPa sqrt(m)) fracture toughness. It also exhibits excellent fatigue life of 180 ksi (1241 MPa) stress at 1x10^7 cycles Run-Out in Axial (R=0.1, Kt=1, 25 Hz) Fatigue. PremoMet® is not a stainless alloy and may require plating or coating with a rust preventative or oil to prevent corrosion.

Type Analysis

  • Carbon (Nominal) 0.4
  • Silicon (Nominal) 1.5
  • Nickel (Nominal) 3.8
  • Manganese (Nominal) 0.9
  • Chromium (Nominal) 1.25
  • Molybdenum (Nominal) 0.5
  • Iron (Nominal) Balance
  • Copper (Nominal) 0.5
  • Vanadium (Nominal) 0.3

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

  • AMS 6482

Bar

Rounds

Billet

Wire