AerMet® 100 Plus

UNS #K92580

AerMet® 100Plus is a modification of the Aermet 100 alloy to enhance the fatigue performance. It maintains the high hardness, strength and exceptional ductility/toughness of Aermet 100 and is designed for components requiring high strength, high fracture toughness and exceptional resistance to stress corrosion cracking and fatigue.

Type Analysis

  • Carbon (Nominal) 0.23
  • Nickel (Nominal) 11.5
  • Chromium (Nominal) 3.1
  • Cobalt (Nominal) 13.5
  • Molybdenum (Nominal) 1.2
  • Iron (Nominal) Balance

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applications

Applicable Specifications

  • AMS 6478
  • AMS 6532
  • McDonnell Douglas MMS 217
  • MIL HDBK-5