AerMet® 360

AerMet® 360 alloy possess higher hardness and strength than the AerMet® 340 alloy. The alloy has a superior toughness to specific strength ratio compared to alloys of equivalent strength. The alloy should be considered as a candidate for use in components requiring ultra-high strength and good fracture toughness.

Type Analysis

  • Carbon (Nominal) 0.33-0.36
  • Phosphorus (Maximum) 0.003
  • Silicon (Maximum) 0.03
  • Nickel (Nominal) 11.0-11.2
  • Titanium (Nominal) 0.008-0.015
  • Manganese (Maximum) 0.04
  • Sulfur (Maximum) 0.001
  • Chromium (Nominal) 1.75-1.85
  • Cobalt (Nominal) 16.90-17.10
  • Molybdenum (Nominal) 2.30-2.40
  • Iron (Nominal) Balance
  • Aluminum (Maximum) 0.015
  • Nitrogen (Maximum) 0.001
  • Oxygen (Maximum) 0.001

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

Bar

Rounds

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.