Biodur® L-605

UNS #R30605

L-605 is a nonmagnetic, chromium-nickel-tungsten-cobalt alloy possessing good oxidation and corrosion resistance as well as high strength properties at elevated temperatures. The high strength properties of this alloy may be obtained through work hardening, and it remains nonmagnetic in this condition. Although the aging response of L-605 is considered minimal when compared to typical age hardening alloys, it may be used in the cold worked and aged condition in certain instances. L-605 is generally melted using vacuum induction melting (VIM), followed by electroslag remelting (ESR). The finished mill product is supplied in the solution annealed or cold worked condition, depending on section size and application.

Type Analysis

  • Carbon (Maximum) 0.05-0.15%
  • Phosphorus (Maximum) 0.03
  • Silicon (Maximum) 0.4
  • Nickel (Nominal) 9.00-11.00
  • Tungsten (Nominal) 14.00-16.00
  • Manganese (Maximum) 1.00-2.00
  • Sulfur (Maximum) 0.03
  • Chromium (Nominal) 19.00-21.00
  • Cobalt (Nominal) Balance
  • Iron (Nominal) 3

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

  • AMS 5537
  • AMS 5796
  • ASTM F90
  • ISO 5832-5
  • AMS 5759F

Bar

Rounds

Billet

Wire

Rod