Core Iron

Core Iron is a premium pure iron capable of providing improved soft magnetic characteristics, superior to Electrical Iron when heat treated in the same manner.

Type Analysis

  • Carbon (Maximum) 0.02
  • Silicon (Maximum) 0.05
  • Nickel (Maximum) 0.05
  • Manganese (Maximum) 0.05
  • Chromium (Maximum) 0.05
  • Iron (Nominal) Balance