CTX-909

UNS #N19909

CTX-909 is a high-strength, precipitation hardenable superalloy which exhibits a low and relatively constant coefficient of thermal expansion over a broad temperature range, high hot hardness and good thermal fatigue resistance. It offers a significant improvement over alloys CTX-1 and CTX-3 due to its excellent combination of tensile properties and stress rupture strength to 1200°F (649°C) in the recrystallized condition combined with the use of common age hardening treatments. CTX-909 alloy is weldable, brazable, and can be chromium plated, but requires a protective coating if exposed to atmospheric conditions above 1000°F (538°C).

Type Analysis

  • Carbon (Maximum) 0.06
  • Phosphorus (Maximum) 0.015
  • Silicon (Maximum) 0.4
  • Nickel (Nominal) 38
  • Titanium (Nominal) 1.6
  • Manganese (Maximum) 0.5
  • Sulfur (Maximum) 0.015
  • Chromium (Nominal) 0.5
  • Cobalt (Nominal) 14
  • Iron (Nominal) Balance
  • Aluminum (Nominal) 0.15
  • Copper (Nominal) 0.5
  • Columbium+Tantalum 4.9
  • Boron (Nominal) 0.012

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

  • AMS 5884
  • AMS 5893

Bar

Flats

Rounds

Shapes

Billet

Strip

Wire

Technical Information

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.