M10

UNS #T11310

M10 is a general purpose, molybdenum-bearing high speed steel possessing excellent wear resistance and cutting properties due to its high vanadium and carbon content. This alloy is electroslag remelted.

Type Analysis

  • Carbon (Nominal) 0.85
  • Silicon (Maximum) 0.3
  • Manganese (Maximum) 0.2
  • Chromium (Nominal) 4
  • Molybdenum (Nominal) 8
  • Iron (Nominal) Balance
  • Vanadium (Nominal) 2

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applications

Applicable Specifications

  • ASTM A600