MagneDur 20-4 alloy is a cobalt-free alloy with semi-hard magnetic properties. It is malleable and ductile, lending itself to the manufacture of strip, foil, and wire.

Type Analysis

  • Carbon (Nominal) 0.01
  • Silicon (Maximum) 0.2
  • Nickel (Nominal) 20
  • Manganese (Maximum) 0.3
  • Molybdenum (Nominal) 4
  • Iron (Nominal) Balance