PowderRange® 17-4

UNS #S17400

PowderRange® 17-4 stainless steel is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness, along with excellent corrosion resistance, up to 600°F (316°C). It has good fabricating characteristics and can be age-hardened by a single-step, low-temperature treatment, which can be chosen to achieve specific strength and toughness combinations. Due to this balanced combination of performance and ease of use in AM, PowderRange® 17-4 for additive manufacturing has been used for a wide variety of applications, including rapid tooling functional components in nearly every market.

Type Analysis

  • Carbon (Maximum) 0.070
  • Phosphorus (Maximum) 0.040
  • Silicon (Maximum) 1.00
  • Nickel (Nominal) 3.00-5.00
  • Manganese (Maximum) 1.00
  • Sulfur (Maximum) 0.030
  • Chromium (Nominal) 15.00-17.50
  • Iron (Nominal) Balance
  • Copper (Nominal) 3.00-5.00
  • Columbium+Tantalum 0.15-0.45
  • Nitrogen (Maximum) 0.10
  • Oxygen (Maximum) 0.10

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

  • ASTM A564/564M

Powder