PowderRange® AlSi10Mg is ideal for components requiring a combination of lightweight, complex geometries with good thermal properties. The combined silicon and magnesium for this alloy offers increased strength and hardness with the flexibility for the material to be spark-eroded, welded, micro shot-peened, polished, and coated if required. Conventionally cast components are heat treated to improve the mechanical properties, for example using the T6 cycle of solution annealing, quenching, and age hardening. This can also be used after the additive build. PowderRange AlSi10Mg has excellent weldability in laser additive manufacturing processes.

Type Analysis

  • Silicon (Nominal) 9.00-11.00
  • Nickel (Maximum) 0.05
  • Titanium (Nominal) 0.15
  • Manganese (Maximum) 0.45
  • Iron (Maximum) 0.55
  • Aluminum (Nominal) Balance
  • Copper (Maximum) 0.05
  • Nitrogen (Maximum) 0.05
  • Oxygen (Maximum) 0.10
  • Tin (Nominal) 0.05
  • Tin (Maximum)0.10
  • Zinc (Maximum) 0.05
  • Scandium (Nominal) 0.20-0.45

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

  • AMS 7018

Powder

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.