PowderRange® CCM is a non-magnetic, cobalt-chromiummolybdenum alloy exhibiting high strength, corrosion resistance, wear resistance, and excellent biocompatibility. This alloy meets the low carbon wrought version of ASTM F 75 Cast Alloy. PowderRange® CCM powder is produced by vacuum induction melting (VIM) followed by nitrogen gas atomization. It has excellent weldability in laser additive manufacturing processes and can be processed with either nitrogen or argon shielding gas. PowderRange® CCM exhibits high strength up to 1112 °F (600 °C) and maintains mechanical properties under a variety of corrosive environments. It can also be used in Magnetic Resonance Imaging (MRI) equipment, as it is non-magnetic. These properties make PowderRange CCM ideal for small biomedical devices where high strength and fatigue resistance are required.

Type Analysis

  • Carbon (Maximum) 0.10
  • Phosphorus (Maximum) 0.020
  • Silicon (Maximum) 1.00
  • Nickel (Maximum) 0.50
  • Tungsten (Nominal) 0.20
  • Titanium (Nominal) 0.10
  • Manganese (Maximum) 1.00
  • Sulfur (Maximum) 0.010
  • Chromium (Nominal) 27.00-30.00
  • Cobalt (Nominal) Balance
  • Molybdenum (Nominal) 5.00-7.00
  • Iron (Maximum) 0.75
  • Aluminum (Maximum) 0.10
  • Nitrogen (Maximum) 0.25
  • Boron (Maximum) 0.010
  • Oxygen (Maximum) 0.10

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applications

Applicable Specifications

  • ASTM F75

Powder

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.