Pyrowear® 61

UNS #K93061

Pyrowear® 61 is a premium quality carburizing steel that offers high core strength, high fatigue strength, high temperature resistance, and high hardenability versus AISI 9310, X53 (AMS 6308), EN36, and other standard carburizable alloys. Its benefits include light weighting of components and increasing power density in applications in aerospace, energy, racing/off-road/mission-critical vehicles, and other industries where weight savings, compactness, high temperature and surface fatigue resistance are valued. The alloy has achieved carburized case hardness of 60-62 HRC but provides ultra-high core properties for demanding applications. The high tempering temperature (900°F/482°F) offers a 400-600°F (204-315°C) increase in thermal stability relative to conventional gear steels. Well suited to low-pressure carburization at high temperature to reduce manufacturing time and expense while providing reliable carburization profiles, Pyrowear® 61 does not require a separate hardening/quenching process.

Type Analysis

  • Carbon (Nominal) 0.15
  • Nickel (Nominal) 9.5
  • Chromium (Nominal) 3.5
  • Cobalt (Nominal) 18
  • Molybdenum (Nominal) 1.1
  • Iron (Nominal) Balance
  • Vanadium (Nominal) 0.08

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

  • AMS 6517
  • D210-13802-1

Bar

Flats

Rectangles

Rounds

Billet

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.