Ti 3Al-8V-6Cr-4Mo-4Zr

UNS #R58640

Ti-3Al-8V-6Cr-4Mo-4Zr is a metastable beta alloy that is heat-treatable to a wide range of strength levels and used when particularly high strengths are needed along with light weight and corrosion resistance. Offers low elastic modules and excellent fatigue resistance. Also known as Ti-3-8-6-4-4, Beta-C TM or ASTM B348 Grade 19, it is one of the easier beta alloys to melt, exhibiting low segregation, and to process, exhibiting good working and heat treating properties.

Type Analysis

  • Carbon (Maximum) 0.05
  • Titanium (Nominal) Balance
  • Chromium (Nominal) 5.50-6.50
  • Molybdenum (Nominal) 3.50-4.50
  • Iron (Nominal) 0.3
  • Aluminum (Nominal) 3.00-4.00
  • Nitrogen (Maximum) 0.03
  • Hydrogen (Maximum) 0.03
  • Oxygen (Maximum) 0.12
  • Yttrium (Nominal) 0.005
  • Zirconium (Nominal) 3.50-4.50
  • Vanadium (Nominal) 7.50-8.50

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

  • AMS 4957 (Bar
  • Wire
  • Cold Drawn)
  • MIL-T 9046 (Sheet
  • Strip
  • Plate)
  • AMS 4958 (Bar
  • Rod
  • STA)
  • MIL-T 9047 (Bars
  • Billets)

Bar

Rounds

Shapes

Ultrabar Precision Bar

Ingot

Strip

Sheet

Wire

Dynalube Coil

Shapes

Smart Coil Titanium Coil

Weld Wire

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.