Ti 6Al-6V-2Sn

UNS #R56620

Ti 6Al-6V-2Sn is a titanium alpha-beta alloy used as a higher strength alternative to standard Ti 6Al-4V because of its elevated alloy content, but that offers lower toughness and ductility.

Type Analysis

  • Carbon (Maximum) 0.05
  • Titanium (Nominal) Balance
  • Iron (Nominal) 0.35-1.0
  • Aluminum (Nominal) 5.5-6.5
  • Copper (Nominal) 0.75
  • Nitrogen (Maximum) 0.04
  • Hydrogen (Maximum) 0.015
  • Oxygen (Maximum) 0.2
  • Vanadium (Nominal) 5.5-6.5
  • Magnesium (Nominal) 1.8-2.2