Trim Rite® is a quench-hardenable martensitic stainless steel that provides a moderately high level of corrosion resistance, hardness up to Rockwell C 51, good cold formability and ease of heat treatment. Hardness capability of 420 but with superior corrosion resistance and ductility. Balanced to be fully martensitic in the hardened condition and magnetic in all conditions, the alloy can be hot worked, cold worked, machined and heat treated using the same equipment and methods used for 410 stainless steel.

Type Analysis

  • Carbon (Maximum) 0.15-0.30
  • Phosphorus (Maximum) 0.04
  • Silicon (Maximum) 1
  • Nickel (Nominal) 0.25-1.00
  • Manganese (Maximum) 1
  • Sulfur (Maximum) 0.03
  • Chromium (Nominal) 13.50-15.00
  • Molybdenum (Nominal) 0.40-1.00
  • Iron (Nominal) Balance

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

  • ASTM A276
  • ASTM A493

Bar

Rounds

Billet

Strip

Wire

Rod

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.