80A

UNS #N07080

80A is a nickel-base, high-temperature alloy containing a high percentage of chromium characterized by excellent creep-resisting properties, high oxidation resistance, and high resistance to fatigue under very arduous conditions. Aluminum and titanium additions serve as hardening agents. 80A is heat treatable using gamma-prime precipitation. The creep-resisting properties of 80A are adversely affected by cold working the alloy following heat treatment, the effect being to cause an increase in the rate creep under given conditions. This has led to failure by rupture in a shortened time at a large elongation. The properties of the alloy may be restored by re-heat treatment.

Type Analysis

  • Carbon (Maximum) 0.06
  • Silicon (Maximum) 0.35
  • Nickel (Nominal) Balance
  • Titanium (Nominal) 2.35
  • Manganese (Maximum) 0.35
  • Sulfur (Maximum) 0.007
  • Chromium (Nominal) 20
  • Cobalt (Nominal) 1
  • Iron (Nominal) 0.75
  • Aluminum (Nominal) 1.25
  • Copper (Nominal) 0.05

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

  • ASME SB637
  • ASTM B637

Bar

Rounds

Billet

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.