A-286

UNS #S66286

A-286 is an iron-base austenitic stainless steel alloy with notched rupture strength superior to any other alloy with comparable high-temperature properties. It is designed for applications requiring high strength and good corrosion resistance at temperatures up to 1300°F (704°C). An advantage of A-286 is that it can be precipitation hardened and strengthened by heat treatment, making a high degree of uniformity in developing maximum strength possible, which can be duplicated application after application.

Type Analysis

  • Carbon (Maximum) 0.08
  • Silicon (Maximum) 1
  • Nickel (Nominal) 24.00 - 27.00
  • Titanium (Nominal) 1.90 - 2.30
  • Manganese (Maximum) 2
  • Chromium (Nominal) 13.50 - 16.00
  • Molybdenum (Nominal) 1.00 - 1.50
  • Iron (Nominal) Balance
  • Aluminum (Maximum) 0.35
  • Boron (Nominal) 0.003 - 0.010
  • Vanadium (Nominal) 0.10 - 0.50

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

  • AMS 5525 (Strip)
  • AMS 5732
  • AMS 5735
  • AMS 5737
  • ASTM A453
  • MR0175
  • AMS 5731
  • AMS 5734
  • AMS 5736
  • AMS 5895
  • ASTM A638