AerMet® 310

AerMet® 310 alloy possesses higher hardness and strength than AerMet® 100 alloy while exhibiting exceptional ductility and toughness. At a 310 ksi (2137 MPa) ultimate tensile strength, it exhibits toughness values equivalent to alloys 20 ksi (138 MPa) lower in strength. The alloy should be considered as a candidate for use in components requiring high strength, high fracture toughness and exceptional resistance to stress corrosion cracking and fatigue.

Type Analysis

  • Carbon (Nominal) 0.25
  • Nickel (Nominal) 11
  • Chromium (Nominal) 2.4
  • Cobalt (Nominal) 15
  • Molybdenum (Nominal) 1.4
  • Iron (Nominal) Balance

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

Bar

Hollow Bar

Rounds

Billet

Plate

Strip

Sheet

Wire

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.