Electrical Iron

Electrical Iron is a low carbon iron with good direct current soft magnetic properties after heat treatment. It is produced using the electric arc melting process. Other elements commonly found in low carbon irons are held as low as possible in order to provide material capable of producing good direct current soft magnetic properties. After a standard magnetic aging treatment, HC from 15 kG increases less than 6% when employing a 1562°F (850°C) forming gas initial heat treatment.

Type Analysis

  • Carbon (Maximum) 0.02
  • Phosphorus (Nominal) 0.01
  • Silicon (Nominal) 0.12
  • Nickel (Nominal) 0.08
  • Manganese (Nominal) 0.12
  • Sulfur (Nominal) 0.01
  • Iron (Nominal) Balance
  • Vanadium (Nominal) 0.04-0.10

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

  • ASTM A848 Alloy 1

Bar

Rounds

Billet

Strip

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.