Custom 450®

UNS #S45000

Custom 450® is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to 304) with moderate strength (similar to 410). The alloy has a yield strength somewhat greater than 100 ksi (689 MPa) in the annealed condition but is easily fabricated. A single-step aging treatment develops higher strength with good ductility and toughness. This stainless can be machined, hot-worked, and cold-formed in the same manner as other martensitic age-hardenable stainless steels with mechanical properties that will depend on the aging temperature selected. A particular advantage is ease of welding and brazing.

Type Analysis

  • Carbon (Maximum) 0.05
  • Phosphorus (Maximum) 0.03
  • Silicon (Maximum) 1
  • Nickel (Nominal) 5.00-7.00
  • Manganese (Maximum) 1
  • Sulfur (Maximum) 0.03
  • Chromium (Nominal) 14.00-16.00
  • Molybdenum (Nominal) 0.50-1.00
  • Iron (Nominal) Balance
  • Copper (Nominal) 1.25-1.75
  • Columbium/Niobium 8 X C Minimum

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

  • AMS 5763
  • AMS 5863 (Strip)
  • ASTM A693 (strip)
  • MR0175
  • AMS 5773
  • ASTM A564 (XM-25)
  • ASTM A959

Bar

Flats

Rounds

Square

Billet

Plate

Strip

Sheet

Wire

Shapes

Weld Wire

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.