Gall-Tough® Plus

UNS #S20162/S21800

Gall-Tough® Plus (Nitronic 60) is a high silicon, high manganese, nitrogen strengthened, austenitic stainless alloy which exhibits superior self-mated galling and metal-to-metal wear resistance. The alloy possesses higher strength and chloride corrosion resistance equal to or better than 316, along with equivalent high temperature oxidation resistance. Gall-Tough® Plus stainless may be considered for applications in which parts are in relative motion under load without lubricants.

Type Analysis

  • Carbon (Maximum) 0.15
  • Phosphorus (Maximum) 0.04
  • Silicon (Maximum) 2.50-4.50
  • Nickel (Nominal) 6.00-10.00
  • Manganese (Maximum) 4.00-8.00
  • Sulfur (Maximum) 0.04
  • Chromium (Nominal) 16.50-21.00
  • Cobalt (Nominal) 0.75
  • Molybdenum (Nominal) 0.50-2.50
  • Iron (Nominal) Balance
  • Nitrogen (Nominal) 0.05-0.25

Downloads

Request a Quote

Applicable Specifications

Bar

Flats

Hexagons

Rounds

Billet

Strip

Sheet

Wire

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.