High Permeability 49

UNS #K94840

High Permeability "49" is a 48% nickel-iron alloy that possesses the highest saturation flux density of any nickel-iron alloy. The saturation flux density of about 16000 gauss (1.6 tesla) combined with its high initial and maximum permeability and low core loss after heat treatment make this a versatile alloy with many potential applications. Available in three grades (standard, rotor grade, and transformer grade), it is ideal for applications requiring extremely high permeability at low magnetizing forces to increases the efficiency and effectiveness of the equipment.

Type Analysis

  • Carbon (Nominal) 0.02
  • Silicon (Nominal) 0.35
  • Nickel (Nominal) 48
  • Manganese (Nominal) 0.5
  • Iron (Nominal) Balance

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

  • ASTM A753 Alloy 2
  • MIL-N-14411B (MR) (Composition 3 and 4)
  • IEC 404-8-6 (Alloy class E3)

Bar

Rounds

Billet

Stacks

Strip

Sheet

Wire

Shapes

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.