Trinamet®

UNS #S42030

Trinamet® is a hardenable martensitic stainless steel with a combination of cold formability, corrosion resistance, and high heat treated hardness. It combines improved corrosion resistance over 410 stainless with a hardness up to 53 HRC and improved formability over 17Cr-4Ni. It can be hot worked, cold worked, machined and heat treated using similar equipment and methods used for 410 stainless steel.

Type Analysis

  • Carbon (Maximum) 0.3
  • Phosphorus (Maximum) 0.04
  • Silicon (Maximum) 1
  • Manganese (Maximum) 1
  • Sulfur (Maximum) 0.03
  • Chromium (Nominal) 12.00-14.00
  • Molybdenum (Nominal) 1.00-3.00
  • Iron (Nominal) Balance
  • Copper (Nominal) 2.00-3.00

New Feature!

Build a list of your favorite alloys. Click the heart icon on any alloy to being creating your account.

Downloads

Request a Quote

Applicable Specifications

Bar

Strip

Wire

Rod

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.